As always I appreciate your experienced input and your understanding of my perspective...wishing to retain the wooden beam appearance. Your suggestion of contacting Gougeon Brothers in Michigan is yet another step for me to take to help me get this right the first time around.
Michael #133----- Original Message -----
From: "Don Campbell" <dk.campbell at sympatico.ca>
To: "Alberg 30 Public List -- open to all" <public-list at lists.alberg30.org>
Sent: Thursday, January 7, 2010 12:06:19 PM GMT -05:00 US/Canada Eastern
Subject: Re: [Public-List] Mast Beam Repair
With the new epoxies like G-flex from Gougeon's, you have better
materials than we had even 2 years ago. G-flex was developed to
overcome the problems with normal epoxies of adherence and strength of
joints with teak and mahagony. G-flex has the strongest modulus of
elasticity of any epoxy in production so far. If you like the look of
oak, you might want to call them in Michigan and ask about the reaction
for red oak . It may make some sense to switch to white oak if there is
better adherence and you would still have a very attractive beam.to look
at. White oak has a better reputation for lasting than red oak and the
really good English white oak will last in soil for 50 years per inch of
heartwood when used in the construction of wooden henges (similar to
Stone Henge but made of wood). There was an interesting article on wood
henges in Scientific American about 35 years ago for that information.
John has mentioned acids in red oak. Normally plants do not have
much of an imbalance of ionic charges so these are organic acids but
strong oxidizers as well . I do know that with red oak particularly,
that if it sits on steel for long as the board is cut from the log on
the sawmill, it turns very black, very quickly. The iron in the steel is
oxidized and the oxide sticks to and discolours the wood. I have never
tried litmus on red oak sap though. If this is the case that there are
acids in the wood, every time it gets wet, there is a replacement of the
hydrogen ion and so the acid reaction continues again, the same way you
add just water to a wet cell battery.
Don #528
>
_______________________________________________
These businesses support your Association:
http://www.alberg30.org/store/A30supporters.html
Please support them.
_______________________________________________
Public-List mailing list
Public-List at lists.alberg30.org
http://lists.alberg30.org/listinfo.cgi/public-list-alberg30.org
1262884473.0
More information about the Public-List
mailing list