Is Lexan what it is? I stand corrected. I don't know my plastics, but
what I have is heavy, tough stuff that is frosted and I can jump up and
down on with impunity. But then, I'm on the small side. Never leaks either.
Bob Kirk
Isobar #181
>If you're going to use some clear plastic for your hatch don't use acrylic!
>Use Lexan or coated Polycarbonate (the same thing). It is much much
>stronger. I challenge you to take a piece of say 1/4 inch acrylic and a
>piece of 1/4 inch polycarbonate of the same dimensions and hit each as
>hard as you can with a hammer. I have done this and I will never go to
>sea with a piece of acrylic on any hatch or port light again.
>
>Hugh Freebairn
>"Aliage"
+---------------------------------------------------------------------------+
| Rough conditions in the Southern Ocean. Read about the brutal challenges. |
| http://service.bfast.com/bfast/click?bfmid=22673860=32743498=bt_challenge |
+---------------------------------------------------------------------------+
_______________________________________________
Public-list mailing list -- Public-list at alberg30.org
http://www.alberg30.org/mailman/listinfo/public-list
To unsubscribe: email to Public-list-request at alberg30.org
Include command "unsubscribe <password>" in subject or body.
Use command "help" for more options.
986436601.0
More information about the Public-List
mailing list