Justin,
406 is silica, right? I would use something lighter. (But not microballoons. They might soak up water under the waterline.)
George
Sent from a primitive pocket computer. Please assume all errors are due to that.
> On May 27, 2016, at 19:13, Justin Riddle via Public-List <public-list at lists.alberg30.org> wrote:
>
> Hi Albergers,
> I've discovered delamination in the rudder.
> https://goo.gl/photos/FB74t3mwGFGCWQ2YA
>
> What sort of coring material do you think would be good to build this back
> up before glassing? I was thinking West System 406 thickened up pretty well.
>
> Thoughts?
>
> Thanks!
> Justin
> Hiraeth #498
> _______________________________________________
> These businesses support your Association:
> http://www.alberg30.org/store/A30supporters.html
> Please support them.
> _______________________________________________
> Public-List mailing list
> Public-List at lists.alberg30.org
> http://lists.alberg30.org/listinfo.cgi/public-list-alberg30.org
More information about the Public-List
mailing list